Surface Preparation第 22 / 100 题

Before applying an elastomeric coating to a stucco crack, what prep step is typically needed?

a.Wetting the crack with solvent
b.Cleaning and filling/bridging the crack and ensuring the surface is sound and dry
c.Applying gloss enamel first
d.Sanding the entire wall to bare masonry

解析

Elastomeric coatings bridge hairline cracks but the substrate must first be clean, sound, and dry, with larger cracks filled or reinforced. Loose material and contaminants would cause the thick coating to fail. Proper prep lets the elastomeric film stretch over the crack without delaminating.

免费刷完整 100 道题库 — 无需注册。

同考点相关题目

最近核对: · 审核流程

PrepPass 编辑团队 · 依据官方资料核对 California CSLB C-33 Painting & Decorating Trade Exam · 我们如何核对
反馈