Core TradesQuestion 121 of 700
Under normal ambient conditions, what is the MINIMUM period that standard structural concrete should be kept continuously moist to develop adequate strength and durability?
a.24 hours
b.3 days
c.7 days
d.28 days
Explanation
Cement hydration continues only while moisture is present, so a continuous moist-cure of at least 7 days is the common minimum for standard mixes. 24 hours and 3 days stop hydration too early and reduce strength and surface durability. 28 days is the age at which design strength is typically verified, not the required curing duration.
Law Reference: 2025 CA Building Code, Chapter 19 (Concrete)Practice all 700 questions free — no signup required.
Related questions on this topic
- In a mixed California climate, a vapor retarder placed on the WRONG side of the insulation can cause:
- CALCULATION: A ceiling requires R-49 insulation. If a certain blown insulation provides R-3.5 per inch, what minimum installed thickness is needed?
- A kickout (diverter) flashing is installed where a roof edge meets a vertical wall at the bottom of a roof-wall intersection. Omitting it commonly causes:
- What is the MINIMUM concrete cover required to protect reinforcing steel in concrete that is cast against and permanently exposed to earth?
- A rectangular slab measures 30 ft by 40 ft and is 4 inches thick. How many cubic yards of concrete are needed (before any waste allowance)?
- Assuming proper placement and curing, which change to a concrete mix will produce the GREATEST increase in compressive strength?
Last reviewed: · editorial process
PrepPass Editorial Team · Verified against California CSLB General Building (B) Trade Examination · How we review