Core TradesCâu 9 / 700
When placing concrete in cold weather, fresh concrete must generally be protected from freezing until it reaches a compressive strength of at least about:
a.100 psi
b.500 psi
c.1,500 psi
d.3,000 psi
Giải thích
Concrete is vulnerable to permanent damage if it freezes before reaching roughly 500 psi, so it must be kept above freezing until that early strength is achieved. 100 psi is too low to resist damage, while 1,500 and 3,000 psi are well beyond the point where freezing is critical.
Trích dẫn luật: 2025 CA Building Code (CBC) Chapter 19 (Concrete)Luyện miễn phí toàn bộ 700 câu hỏi — không cần đăng ký.
Câu hỏi liên quan cùng chủ đề
- Which curing method retains moisture in fresh concrete by forming a sealing film on the surface after finishing?
- A No. 5 reinforcing bar has a nominal diameter of 5/8 inch. If the specified tension lap splice is 40 bar diameters, what is the MINIMUM lap length?
- For a typical residential interior slab-on-ground, what is a common MINIMUM slab thickness?
- During hot-weather concreting, plastic shrinkage cracking is BEST prevented by:
- Six cylindrical concrete piers are each 18 inches in diameter and 4 feet deep. Approximately how many cubic yards of concrete are needed for all six?
- A rectangular slab measures 20 feet by 25 feet and is 5 inches thick. Approximately how many cubic yards of concrete does it require?
Cập nhật gần nhất: · quy trình kiểm tra
Đội Ngũ Biên Tập PrepPass · Đối chiếu với California CSLB General Building (B) Trade Examination · Quy trình kiểm tra